The buyer decision
Do not approve a replacement wheel for acidic cleaning solely because both wheels are called polyurethane (PU). For 10% aqueous citric acid, TENTE rates PU as conditionally resistant; Blickle lists its polyester- and ether-based PU families as resistant; Schwalb lists generic PU as not suitable. The safe conclusion is not that one supplier is correct for every wheel. It is that generic PU is too broad a specification to establish compatibility.
What the manufacturers actually publish
| Manufacturer / source | 10% citric-acid entry | Rating meaning and scope |
|---|---|---|
| TENTE | Catalogue 8.0, printed p.36: rubber ++, polyamide +, polyurethane +; diluted citric acid 10% | ++ resistant; + conditionally resistant; = non-resistant. Broad material classes; no shared exposure protocol is stated in the table. |
| Blickle | Current “Environmental factors” table: 10% aqueous citric acid is + for rubber, TPE, nylon, PP Copo, polyester PU families and ether PU families, and stainless steel AISI 304 | + resistant; 0 resistant under certain conditions; x not resistant. It separates polyester and ether PU families, but does not provide a matched finished-wheel test protocol for this row. |
| Schwalb Castors | Current “Chemical resistance” table: 10% aqueous citric acid; polyamide suitable, polyurethane not suitable, Vulkollan not specified, rubber suitable | Legend: suitable / limited suitability / not suitable / not specified. Where no special information is given, standard commercial purity/concentration and room temperature are assumed. |
The difference is material: Schwalb's “not suitable” for PU is more restrictive than TENTE's “conditionally resistant” and Blickle's “resistant”. The sources are independent caster manufacturers, not reposts of one common table.
Why the three ratings cannot be ranked as if they were one test
- The rating scales differ. TENTE uses ++ / + / =; Blickle uses + / 0 / x; Schwalb uses suitable / limited / not suitable / not specified. A plus sign does not mean the same thing across all three systems.
- The material labels are not identical. Blickle separates polyester-based PU families from ether-based PU families. TENTE and Schwalb use broader polyurethane columns in the cited tables. A generic PU column does not identify a specific formulation or cast/thermoplastic process.
- The stated exposure conditions are incomplete and differ. TENTE says contact duration, concentration, humidity and temperature affect material response and that its table does not apply to mixtures. Blickle likewise says concentration, contact duration, temperature, humidity and mixtures matter. Schwalb states a default of standard commercial purity/concentration and room temperature when no special condition is given; its table is based on tests, raw-material-supplier recommendations and customer reports.
- There is no common test protocol. The cited entries do not share a declared specimen geometry, dwell time, immersion/spray/wipe exposure, number of cycles, mechanical load or acceptance criterion. No matched cross-brand comparison was found.
Hamilton's chart is a useful warning, not a fourth 10% data point
Hamilton Caster's Chemical Resistance Chart (copyright 2020, PDF p.2) lists “Citric Acid” without a concentration. Its key defines D as “Severe Effect or Not Recommended”; the row gives polyurethane D, Nylast B, Aqualite B and Scorcher A. This reinforces that the exact wheel-material family matters, but the missing concentration means it cannot be compared with the three 10% aqueous-citric-acid entries above.
Hamilton's 2020 article identifies four application variables: exposure frequency (intermittent or continuous), exposure type (immersion, atomized spray or roll-through), chemical concentration and physical/dynamic performance requirements. It also says the chart is a guide and recommends testing under actual conditions. This is a useful RFQ checklist, not evidence that the Hamilton chart and the other manufacturers used the same protocol.
What this changes in selection and substitution
For a buyer using a 10% citric-acid descaler, a generic “PU wheel” should be classified as not yet qualified until the exact wheel maker confirms the actual compound and exposure. A more permissive chart is not a substitute for that confirmation; a more restrictive chart should not be silently ignored. If the original and replacement wheels come from different manufacturers, preserve the manufacturer/model attribution and ask both suppliers against the same cleaning sequence.
RFQ and first-article acceptance questions
- Provide the exact cleaner trade name, technical data sheet or safety data sheet, active ingredients, in-use dilution and concentration basis.
- State solution temperature, pH if supplied by the cleaner maker, exposure type (wipe, splash, spray, roll-through or immersion), contact/dwell time, frequency per shift/week and rinse/dry procedure.
- Identify the wheel manufacturer, exact model, tread compound/trade name, polyester/ether chemistry if disclosed, cast or thermoplastic process, wheel-core material and any tread-to-core bonding system.
- Confirm whether the wheel is parked under load during cleaning, rolls while wet, or is cleaned after a loaded operating cycle; state the per-wheel load, speed and turning duty.
- Obtain written compatibility confirmation for the exact model and exposure. If evidence remains conflicting, agree a sample/first-article trial with repeat cycles and acceptance criteria before fleet substitution.
- Inspect the complete caster separately: hub, axle, wheel bearing, bearing seals, grease, swivel head, bracket coating, fasteners and brake materials may have different exposure limits. A tread-material chart does not qualify all these components.
- Define acceptance checks such as swelling, softening, cracking, tackiness, dimensional/hardness change, tread-to-core separation and retained rolling/load function. These are proposed buyer checks, not a claim that the cited manufacturers use one standard test.
Evidence and source locations
- TENTE, Catalogue 8.0 — Castors & Wheels, edition 8.0 (1/2023), printed p.36, “Analysis of the Chemical Resistance” and material table: diluted citric acid 10%; rubber ++, polyamide +, polyurethane +; legend ++ resistant / + conditionally resistant / = non-resistant. Original catalogue PDF.
- Blickle, “Environmental factors”, current manufacturer guide accessed 2026-11-25, “Chemical resistance” table: 10% aqueous citric acid; separate polyester PU and ether PU columns; legend and exposure caveats. Original manufacturer guide.
- Schwalb Castors, “Chemical resistance”, current manufacturer technical page accessed 2026-11-25, row “citric acid, aqueous 10%”; suitable/limited/not suitable/not specified legend; default room-temperature assumptions and evidence basis. Original manufacturer table.
- Hamilton Caster, Chemical Resistance Chart, copyright 2020, PDF p.2, “Citric Acid” row: concentration not stated; polyurethane D, Nylast B, Aqualite B, Scorcher A; key A excellent / B good / C fair to poor / D severe effect or not recommended. Original chart PDF.
- Hamilton Caster, “Just how compatible are Hamilton wheels in the chemical world?”, 2020-07-30, paragraphs 4–6: exposure frequency, exposure type, concentration, dynamic requirements and limitations of the chart. Original manufacturer article.
Evidence limits
The sources establish a real disagreement in manufacturer guidance, but they do not resolve it experimentally. The cited tables do not provide a common formulation, test temperature, exposure duration, repeated-cycle schedule, mechanical load or acceptance threshold. Schwalb does not identify the exact PU formulation in its broad column; TENTE's PU is also a broad category; Blickle's finer polyester/ether split still does not disclose a common finished-wheel test protocol for the 10% row. Hamilton's concentration-free citric-acid entry cannot resolve the 10% case. Commercial descalers may contain blends or additives, so a pure citric-acid row cannot qualify an unknown mixture.
No citric-acid compatibility, washdown-cycle, wheel-bearing, seal or complete-caster test has been performed on products supplied by this business. No supplier-specific acid-resistance rating, certification or service-life guarantee is claimed.